TITANE & Alliages (Titan)
Gr2 T40 (CP), Gr4 T60, Gr5 TA6V (6Al4V & Medical ELI),
TA3V (TA3V2,5), TA6ZRD (IMI685 & 662), TA6ZR4DE (6242), 10-2-3,
TA5E, TA8DV, TA5CD4 (Ti17), TU2 (IMI230)...

NICKEL & Alliages (Nickel)
NC20T (alloy 75), NC15Fe (alloy 600), NC22DNb (alloy 625),
NC19FENb (alloy 718), NC15FET (alloy x750), Alloy 800 (32-20),
Alloy 825 (40-38-3), Z8NCDT42 (alloy 901),
ND16CWA (alloy C276, C4, C22, C2000) NC22FED (alloy X),
NCK20D (C 263), CNKDW20 (N 155), NC20K14 (Waspalloy)...

BASE Cobalt (Stelitte)
KC20WNX (St 25), KCN22W (St 188), MP35...

ALUMINIUM (Aluminium)
2017-2024-2618-5086-6061-7075...

ACIERS SPECIAUX (Special steels)
15CDV6 - 35NCD16 - 35NC6 - 40NCD16 - 16NCD13...
Z12CNDV12 (X13VD),
Z15CNU17 (17/4/Ph),
Z15CND17-3 (APX2), Z8CND17-4 (APX4),
Z10CKD10, EZ2NKD18 (Maraging 250)...

ACIERS Inoxydables (Stainless steels)
EZ6NCT25 (A286),
Z10CNW17 (alloy ns190), Z25CNWS20 (X20T),
Z6CNd18-10 (aisi 302-304-309-310-316-317-321-347),
Uranus B6 (aisi 904), 254SMO,
Z100CD17, Z10CF17 (aisi 430),
Z12,30,200 C13 (aisi 410-420)...

ALLIAGES coulés (Castings)
Alloy 100 - 713 - 738 - René 44 - 77 - 125...

 
Toutes ces nuances se déclinent pour les produits :
> Feuillards, Tôles, Plats :
épaisseur de 0.3 mm jusqu’à 100 mm
> Fils & barres :
diamètre de 1 mm à 400 mm
> Tubes & ébauches :
diamètre ext. de 2 mm à 300 mm.
Semi-products Dimensions :
> Coils, sheets, plates :
thickness from 0.3 mm to 100 mm
> Wire & bars :
diameter from 1 mm to 400 mm
> Tubes & pipes :
OD. from 2 mm to 300 mm.